Re: Exposed Aggregate Bench ColumnsFrom: hawkeye1201@yahoo.com Comments7 aggregate to 1 portland is the usual ratio. I would probably do 2 sand 5 pea and 1 portland. I think you will also need to apply a retarder to the forms if you expect to expose the aggregate the next day. You could do a test pour to see if that works to your satisfaction.
|
|